MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lehvoss LUVOCOM® 3F TPU CNT 9902 BK TPU for Additive Manufacturing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Thermoplastic polyurethane with CNT, electrically conducting, black

Main features: For dynamic stress and wear resistance Suitable for discharging of statically-generated electricity.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc1.25 g/ccISO 1183-3
Water Absorption <= 0.300 %
@Time 86400 sec
<= 0.300 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.00900 - 0.0170 cm/cm0.00900 - 0.0170 in/inDIN 16742
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 24.0 MPa3480 psi50 mm/min; ISO 527
Elongation at Break 220 %220 %50 mm/min; ISO 527
Tensile Modulus 0.0400 GPa5.80 ksi1 mm/min; ISO 527
Charpy Impact Unnotched NBNB80x10x4mm; ISO 179 1eU
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+11 ohm<= 1.00e+11 ohmRonde 60x4mm; DIN EN 62631-3-2
Insulation Resistance <= 1.00e+11 ohm<= 1.00e+11 ohmstrip electrode R25; DIN EN 62631-3-3
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air  90.0 °C
@Time 7.20e+7 sec
194 °F
@Time 20000 hour
Continuous; IEC 60216
 110 °C
@Time 720000 sec
230 °F
@Time 200 hour
during lifetime
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 200 - 240 °C392 - 464 °F
Zone 1 190 - 230 °C374 - 446 °F
Zone 2 190 - 230 °C374 - 446 °F
Zone 3 190 - 230 °C374 - 446 °F
Mold Temperature 25.0 - 60.0 °C77.0 - 140 °F
Drying Temperature  60.0 - 90.0 °C
@Time 7200 - 10800 sec
140 - 194 °F
@Time 2.00 - 3.00 hour
Dehumidifying
 100 - 110 °C
@Time 7200 - 10800 sec
212 - 230 °F
@Time 2.00 - 3.00 hour
Vacuum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUU8740 / 325124

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.