MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Moplen HP3841 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Moplen HP3841 is a polypropylene homopolymer used for extrusion applications. Moplen HP3841 has a very narrow molecular weight distribution and is formulated with an anti-gasfading stabilization package. Moplen HP3841 is used for the production of continuous filaments. Typical applications are high tenacity yarns (HTY) and spunbond nonwovens. The grade being in development, this is a preliminary datasheet subjected to changes after product industrialization. This grade is not intended for medical and pharmaceutical applications.

Status: Developmental

Availability: Africa-Middle East; Asia-Pacific; Europe

Application: Filament Yarn; Geotextile & Agriculture; Hygiene Nonwoven

Market: Textile

Processing Method: Continuous Filament/Spinning; Injection Molding; Spunbond

Attribute: Homopolymer; Narrow Molecular Weight Distribution

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 25.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
25.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psiISO 527-1, -2
Tensile Strength, Yield 33.0 MPa4790 psiISO 527-1, -2
Elongation at Break >= 50.0 %>= 50.0 %ISO 527-1, -2
Elongation at Yield 11.0 %11.0 %ISO 527-1, -2
Flexural Modulus 1.25 GPa181 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FUnannealed; ISO 75B-1, -2
Vicat Softening Point 151 °C304 °FA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEQS9697 / 324632

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.