MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik Kanthal Super ER Molybdenum disilicide
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Kanthal Super ER is a new electric heating element with the unique ability to operate up to 1580°C (2875°F) directly in a wide range of furnace atmospheres from very dry reducing to oxidizing. With Kanthal Super ER heating elements it is possible, in just one furnace, to operate firing cycles where the atmosphere condition can be altered, during the cycle, between oxidizing, inert, carburizing, nitriding, reducing and rough vacuum. The major reason for the new and outstanding features of Kanthal Super ER heating elements is that it has a protective surface of pure alumina. The alumina layer grows on the surface of the heating element at high temperatures even in dry hydrogen. The elements can work in direct contact with high alumina supports without corrosive reactions. Kanthal Super ER heating elements cover a wide range of furnace atmospheres and processes. Most types of PM sintering in dry hydrogen and furnace with alternating oxidizing and reducing atmospheres. Continuous furnace with hydrogen atmospheres for ferrite sintering and MLCC processing.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1580 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5030 / 199594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.