MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Silicones UltraGlaze SSG4000AC Accelerated Cure Silicone Structural Glazing Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: UltraGlaze SSG4000AC structural glazing adhesive is a one-component, high-strength neutral cure silicone elastomeric adhesive with accelerated cure characteristics providing for enhanced early hour cure properties. SSG4000AC is useful in structurally glazed curtain wall applications. The material is supplied as a paste, which cures into a durable flexible silicone rubber upon exposure to atmospheric moisture.

Features: Silicone durability, Stable consistency (uncured state), Thermal stability (cured state), Primerless adhesion, Low sag or slump, Accelerated cure, High tensile strength, High tear strength, Compatible with these GE sealants insulating glass products: IGS3703, IGS3713-D1, IGS3729, IGS3723, IGS3733. Compatible with these GE sealants weatherproofing sealants: SCS2000, SCS2700, SCS9000, SCS2800 series. Compatible with these GE sealants SSG products: SSG4000AC structural glazing adhesive and SSG4800J, SCS2000, SSG4400 series. Non-corrosive cure byproduct with low odor.

Applications: structural glazing applications such as factory glazing of unitized curtainwall systems or in field constructed stick curtainwall systems. Use as a weatherseal product, when movement expected in the joint does not exceed its movement capability (±25%). Useful as a bedding material in the fabrication of doors and windows. SSG4000AC has been validated in designs as an appropriate candidate for consideration for use in protective glazing applications. Useful in panel stiffener applications.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccUncured.
Volatile Organic Compounds (VOC) Content 37 g/lUncured.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 33ASTM D2240
Tensile Strength, Ultimate 1.03 MPaASTM C1135
 2.14 MPaASTM D412
Tensile Stress at Strain 0.370 MPa
@Strain 25 %
ASTM C1184
 0.580 MPa
@Strain 50 %
ASTM C1184
Elongation, Ultimate 155 %ASTM C1135
 433 %ASTM D412
Shear Strength 0.800 MPa
@Thickness 6.35 mm
ASTM C961
Tear Strength 11.73 kg(f)/cmDie B.; ASTM D624
Peel Strength 37.8 pli
@Temperature 23.9 °C,
Time 1.81e+6 sec
Aluminum glass. 50% RH; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -55.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 168 - 240 hourFull cured. Most common bead sizes.
 24.0 - 48.0 hour
@Temperature 24.0 °C
1/4" deep section. 50% RH
Tack-Free Time 60.0 - 90.0 minASTM C679
Working Life 10.0 - 20.0 min
 
Descriptive Properties
AppearancePaste
Application Rate2 secondsASTM C603.
ColorBlack, grayUncured.
Consistency / Sag0.1" maxASTM D2202
Joint Movement Capability+/- 25%ASTM C719.
Silicone Content (%)100Uncured
UV & Weathering ResistanceExcellentGE 20 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9917 / 265727

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.