MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Henkel Loctite® Tak Pak® 444 Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Cyanoacrylate Bonding Adhesives and Gasketing and Wire Tackers
Loctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.

Loctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazards. Loctite offers both Form-in-place (FIP) and Cure-in-Place (CIP) compression gasket materials.

Loctite® Tak Pak Adhesives are used to secure wires to printed circuit board assemblies. The fast cure times of these adhesives help increase the throughput of the wire tacking assembly process.

Loctite® 444 General Purpose Ethyl Tak Pak™ Instant Adhesive
An adhesive designed for printed circuit board assembly and repair. Cures instantly with Tak Pak® Accelerator. Used to tack jumper wires and wires to coil forms. Tamper-proof adjustable components. Mounting standoffs, edge guides and stiffeners to circuit boards. Cure Type: Accelerator Bonding Type: Ethyl cyanoacrylate Commercial item std. A-A-3097 Type II, Class 3 Typical Use: Tak Pak® Wire tacking adhesive

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Viscosity 700 cP700 cP
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 22.1 MPa3200 psiGrit blasted steel
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.500 min0.00833 hour
 1440 min24.0 hourFull Cure; Varies with substrates
 
Descriptive Properties
ColorClear
Gap Fill0.007 in.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
Aptek 2120 PMF Low modulus urethane staking compound
Aptek 2100-A7C/B Low modulus urethane staking compound
Tra-Con Tra-Bond 2116 Low Vapor Pressure Epoxy Staking Compound
Tra-Con Tra-Bond 2112 Rigid Epoxy Staking Compound

PLOCT193 / 51929

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.