MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ChevronTexaco FM ISO 460 Lubricating Oil
Categories: Fluid; Lubricant

Material Notes: Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubricating Oils FM provide performance well above that found in typical white mineral oils often used in the food industry. They contain a special biocide to prevent growth of molds when the product comes in contact with food or water.

Applications

  • Gear sets
  • rotary steamers
  • valves up to 175°C (350°F)
Key Words: CPS Number: 232106; MSDS Number: 6859
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 29.2 °
Viscosity Measurement 118Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 2308 SUS
Saybolt Viscosity at 210°F 169 SUS
Kinematic Viscosity at 40°C (104°F) 437 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 34.7 cStASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.430 mm
 
Thermal PropertiesOriginal ValueComments
Pour Point -9.00 °CASTM D97
Flash Point 243 °CASTM D92
 
Descriptive Properties
Rust preventative Test Procedure BPassSynthetic Sea Water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Aero SAE 60/Grade 120 Engine Oil Uncompounded
ChevronTexaco ISO 680 AIO
ChevronTexaco Gear Compounds EP, ISO 1000
ChevronTexaco Delo® SAE 85W-140 Gear Lubricant ESI®
ChevronTexaco Delo® 400 SAE 50

WCHEV110 / 74725

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.