MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polyram RamTough RZ720 Polycarbonate, UV Stabilized
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: UV stabilized and impact modified polycarbonate for injection molding applications

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53479
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
Melt Flow 15 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 60.0 MPaASTM-D638
Elongation at Break >= 95 %ASTM-D638
Flexural Strength >= 90.0 MPaASTM D790
Flexural Modulus >= 2.20 GPaASTM-D790
Izod Impact, Notched 6.00 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 130 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) >= 120 °CDIN 53461
Vicat Softening Point 145 °CASTM-D1525
Flammability, UL94 V-2
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
Polyram RamTough PZ740 Polycarbonate, UV Stabilized
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14096 GY1200-14 PC, special filler, UV stabilized
Mocom (ALBIS) ALCOM® LD PC 1000 UV 14012 GY1016-14 PC, special filler, UV stabilized

PPOLYRA311 / 57573

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.