MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Rayon ACRYPET IR K304 001 PMMA Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Impact Modified, Molded

Material Notes: Balanced impact strength, molding property, and heat resistance.

Typical Products: Visor, outer pillar of automobile.

Information provided by Mitsubishi Rayon Co.,Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccISO 1183; JIS K7112
Water Absorption 0.30 %
@Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cmMRC method
Melt Flow 3.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
Spiral Flow 150 cm
@Thickness 2.00 mm,
Temperature 250 °C
MRC method
 270 cm
@Thickness 2.00 mm,
Temperature 250 °C
MRC method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 80ISO 2039
Tensile Strength 65.0 MPa1A/5; ISO 527
Elongation at Break 19 %1A/5; ISO 527
Modulus of Elasticity 2.30 GPa1A/1; ISO 527
Flexural Strength 98.0 MPaISO 178
Flexural Modulus 2.40 GPaISO 178
Izod Impact, Unnotched (ISO) 2.90 kJ/m²1A; ISO 180
Charpy Impact Unnotched 43.0 kJ/m²11eU; ISO 179
Charpy Impact, Notched 2.60 kJ/m²1eA; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1e+12 ohm-cmJIS K6911
Surface Resistance >= 1.00e+16 ohmJIS K6911
Dielectric Constant 3.7
@Frequency 60 Hz
JIS K6911
Dielectric Strength 20.0 kV/mm4kV/sec; JIS K6911
Dissipation Factor 0.050
@Frequency 60 Hz
JIS K6911
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CASTM D696
Specific Heat Capacity 1.50 J/g-°CJIS K7123
Thermal Conductivity 0.200 W/m-KASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CISO 75
Vicat Softening Point 98.0 °C
@Load 5.10 kg
ISO 75
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49
@Wavelength 587.6 nm
nd; ASTM D542
Haze 0.50 %
@Thickness 3.00 mm
ISO 14782
Transmission, Visible 92 %
@Thickness 3.00 mm
ISO 13468
 
Descriptive Properties
Arc Resistanceno trackJIS K6911

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Rayon ACRYPET MD 001 PMMA Resin
Mitsubishi Rayon ACRYPET VR S40 001 PMMA Resin
Mitsubishi Rayon Acrypet® VH-001 Heat Stabilized PMMA
Aluminum 6082-T6
Mitsubishi Rayon ACRYPET IR S404 001 PMMA Resin

PMITS9911 / 185886

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.