MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
HB Chemical Cilbond® 48 Bonding Agent
Categories: Other Engineering Material

Material Notes: Cilbond 48 is a one-component bonding system for hot and cold-cure PU’s and TPU’s to all metals during the curing process at temperatures of 68°F to 275°F for cast elastomers and up to 390°F for TPU’s. Cilbond 48 will also bond PU and TPU to epoxies and fiberglass reinforced plastics, polyamides and other engineering thermoplastics, such as Hytrel® PBT, PET, PPS, PPO, PEEK PES etc.

Information provided by HB Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 - 0.920 g/cc
Solids Content 18.1 %
Volatiles 78.5 %
Viscosity Measurement 13 - 17
@Temperature 25.6 °C
[sec], No 3 Zahn Cup
 25
@Temperature 25.6 °C
[sec], DIN 4 Cup
 
Thermal PropertiesOriginal ValueComments
Flash Point 28.4 °FAbel Pensky
 
Processing PropertiesOriginal ValueComments
Mold Temperature 68.0 - 275 °FCast Elastomers
 300 - 445 °FTPU
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceColorless Liquid
Content0.177HAP
Typical Coverage610 ft2/US galat 1 mil dry coating thickness
VOC0.785

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBCHEM028 / 317447

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.