Butanox M-50A is the phthalate-free work horse in GRP curing systems. Medium-reactive, general purpose methyl ethyl ketone peroxide (MEKP) with guaranteed low water content, used for curing unsaturated polyester resins in the presence of a cobalt accelerator at room and elevated temperatures. CAS number: 1338-23-4 EINECS/ELINCS No.: 215-661-2 Applications: Butanox M-50A is a multipurpose catalyst for the room temperature cure of promoted unsaturated polyester resins. Unpromoted unsaturated polyester resins can be heat-cured with Butanox M-50a in the temperature range of 100-127°C. Butanox M-50A also has a high MEKP monomer content which may provide faster gel times in some resin systems. Information provided by Nouryon |