MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Veradel® 3000RP Polyethersulfone (PESU), High molecular weight with a low level of functionality
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersing into solutions and to improve adhesion to substrates when used as a coating.

Veradel® 3000RP r-PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of r-PESU are transparent and have additional desirable properties, including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance.

Veradel® r-PESU polymers are available in two molecular weight regimes. Veradel® 3000RP is a high molecular weight sulfone polymer with a relatively low level of functionality while Veradel® 3600RP has a lower molecular weight sulfone polymer (approximately half the molecular weight of the Veradel® 3000RP) with roughly 3-5 times higher level of functionality. The differences in molecular weight results in highly varied levels of viscosity, when measured under similar conditions.

Typical applications include high-temperature coating formulations and specialty adhesives.

All Veradel® r-PESU polymers are produced at Solvay's state-of-the-art, world-scale facility in Panoli, India under ISO 9001:2000 and ISO 14001:2004 certified quality management systems.

Applications: Adhesives; Cast Film; Coating Applications

Features: Acid Resistant; Chemical Resistant; Creep Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Molecular Weight; High Tensile Strength; Hydrolysis Resistant; Low Flow; Medium Rigidity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 250 µm250 µm
Viscosity 700 - 5000 cP700 - 5000 cPSolution Viscosity; ASTM D445
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiASTM D638
Elongation at Yield 6.5 %6.5 %ASTM D638
Tensile Modulus 2.70 GPa392 ksiASTM D638
Flexural Strength 2.60 MPa377 psiASTM D790
Flexural Modulus 2.60 GPa377 ksiASTM D790
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 220 °C428 °FASTM E1356
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorTransparent - Slight Yellow
FormsGranules; Powder
ProcessingCast Film; Coating; Solution Processing; Spraying

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4585 / 280385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.