MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Mobil Delvac 15W-40 1300 Super
Categories: Fluid; Lubricant

Material Notes: Mobil Delvac 1300 Super 10W-30 and 15W-40 are extra high performance diesel engine oils that help extend engine life in the most severe on and off highway applications. The advanced chemistry of these products delivers exceptional performance in both modern, high-output, low-emission engines including those with Exhaust Gas Recirculation (EGR), as well as older engines operating on low or higher sulfur fuel. As a result, these products exceed the API CI-4 (10W-30) and API CI-4 Plus (15W-40) service categories and JASO DH-1 industry specifications. Mobil Delvac 1300 Super 10W-30 and 15W-40 are recommended for use in a wide range of heavy duty applications and operating environments found in the trucking, mining, construction, quarrying, and agricultural industries. These products will provide outstanding protection in the most demanding diesel engines of Caterpillar, Cummins, Detroit Diesel, Mack, Mercedes Benz, Navistar, Volvo, and others. Mobil Delvac 1300 Super 10W-30 and 15W-40 also meet the API SL specification for gasoline engines and mixed fleets. The outstanding performance reserve of Mobil Delvac 1300 Super 10W-30 and 15W-40 is the result of extensive cooperative development work with major OEMs and advanced additive chemistry with patented Trimer technology. These enhancements assure excellent control of oil thickening due to soot buildup and exposure to higher temperatures and provide outstanding resistance to oxidation, corrosion, wear, and high temperature deposits.

Recommended for use in high performance diesel applications including the latest turbo-charged, low emission engines designs, including those featuring EGR technology; On highway applications operating in both high speed/high load and short haul pick-up/delivery; Off highway applications operating in severe low speed/heavy load conditions; Recommended for use in high performance gasoline engines and mixed fleet operators; Diesel-powered equipment from American and Japanese OEMs; On highway heavy duty trucking and off highway including: construction, mining, quarrying, and agriculture; Transmissions requiring Allison C-4 (SAE 15W-40 Grade)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.879 g/cc
@Temperature 15.0 °C
0.0318 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity  4.3 cP
@Temperature 150 °C
4.3 cP
@Temperature 302 °F
High Temperature High Shear (HTHS); ASTM D4683
 6000 cP
@Temperature -20.0 °C
6000 cP
@Temperature -4.00 °F
CCS; ASTM D5293
 29000 cP
@Temperature -25.0 °C
29000 cP
@Temperature -13.0 °F
MRV; ASTM D4684
Viscosity Measurement 133133Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 123 cSt123 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.6 cSt15.6 cStASTM D445
Ash 1.3 %1.3 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesMetricEnglishComments
Total Base Number 1212mg KOH/g; ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -30.0 °C-22.0 °FASTM D97
Flash Point 230 °C446 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Mobil 1 5W-30
ExxonMobil Mobil 1 0W-40
ExxonMobil Mobil 1 0W-20

WEXXON002 / 75427

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.