MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos ABS Lustran® 308 ABS, Medical Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Lustran® ABS 308 resin is a low gloss, easy-flowing grade of ABS (acrylonitrile butadiene styrene). This injection molding grade offers a good balance of rigidity, impact strength, and abuse resistance. The resin is available in natural (000000). Lustran® ABS 308 resin is designed for applications requiring a good balance of physical properties and a low-gloss appearance. Typical applications include components of intravenous (IV) systems, diagnostic test kits, and surgical instruments. As with any product, use of Lustran® ABS 308 resin in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Lustran® ABS 308 resin is designated as “medical-grade” and has met the requirements of the FDA-Modified ISO 10993, Part I “Biological Evaluation of Medical Devices” tests with human tissue contact time of 30 days or less. Regrind must not be used in medical applications requiring biocompatibility.

Lustran® is now a product of INEOS Styrolution. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM-D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM-D955
Melt Flow 7.0 g/10 min
@Load 3.80 kg,
Temperature 230 °C
Rate; ASTM-D1238
 21 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Index; ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM-D785
Tensile Strength, Yield 36.0 MPaASTM-D638
Tensile Modulus 2.20 GPaASTM-D638
Flexural Yield Strength 72.0 MPaASTM-D790
Flexural Modulus 2400 MPaASTM-D790
Izod Impact, Notched 171 J/m
@Thickness 3.20 mm
ASTM-D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CASTM-D696
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
@Thickness 3.20 mm
Unannealed; ASTM-D648
 92.0 °C
@Thickness 12.7 mm
Unannealed; ASTM-D648
 100 °C
@Thickness 3.20 mm
Annealed; ASTM-D648
 102 °C
@Thickness 12.7 mm
Annealed; ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
@Thickness 3.20 mm
Unannealed; ASTM-D648
 87.0 °C
@Thickness 12.7 mm
Unannealed; ASTM-D648
 95.0 °C
@Thickness 3.20 mm
Annealed; ASTM-D648
 100 °C
@Thickness 12.7 mm
Annealed; ASTM-D648
Vicat Softening Point 106 °CRate B; ASTM-D1525
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 235 - 250 °CInjection Molding
Middle Barrel Temperature 240 - 255 °CInjection Molding
Front Barrel Temperature 245 - 260 °CInjection Molding
Nozzle Temperature 245 - 260 °CInjection Molding
Melt Temperature 245 - 265 °CInjection Molding
Mold Temperature 45.0 - 65.0 °CInjection Molding
Drying Temperature 71.0 - 77.0 °C
@Time 14400 sec
 82.0 - 88.0 °C
@Time 7200 sec
Moisture Content <= 0.10 %
Dew Point <= -29.0 °Cinlet air
Injection Pressure 10000 - 16000 psiInjection Molding
Back Pressure 50.0 - 100 psiInjection Molding
Clamp Pressure 30.8 - 61.6 MPaInjection Molding
Cushion <= 0.250 inInjection Molding
 
Descriptive Properties
Hold Pressure50-75% of Injection Pressure, Injection Molding
Injection SpeedHighInjection Molding
Screw Compression Ratio2.5:1Injection Molding
Screw Length-to-Diameter Ratio>= 20:1Injection Molding
Screw SpeedModerate, Injection Molding
Shot Weight-to-Machine Capacity Ratio0.5-0.75Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Lustran® 308 NR Acrylonitrile Butadiene Styrene (ABS)
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
Covestro Bayblend® FR3010 HF PC/ABS Blend
Covestro Makroblend® UT305 PC/PET Blend
Geon® Performance Solutions Vinyl Flexible XV3855 Polyvinyl Chloride, Flexible

PINEA917 / 107188

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.