MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrofol® BL 6-2 820802 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Characterization: Makrofol BL 6-2 820802 is a virtually glare free, scratch resistant, black translucent extrusion film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol BL 6-2 820802 typical applications are automotive instrument panels, illuminated gauges, dials and graphics, front panels and scales on radios and control consoles, and diffusors on projection screens. Makrofol BL 6-2 820802 is available in a standard thickness of 0.008 ” (200 microns). Other thicknesses are available on request. The surface combination of Makrofol BL 6-2 820802 is one side fine velvet and one side very fine matte. As with any product, use of Makrofol BL 6-2 820802 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.35 %
@Time 86400 sec
0.35 %
@Time 24.0 hour
immersion; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiASTM D882
Elongation at Break 70 %70 %ASTM D882
Tensile Modulus 2.69 GPa390 ksiASTM D882
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 20.0 - 120 °C
22.2 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
CTE, linear, Transverse to Flow 40.0 µm/m-°C
@Temperature 20.0 - 120 °C
22.2 µin/in-°F
@Temperature 68.0 - 248 °F
DIN 53752
Shrinkage  <= 0.20 %
@Temperature <=90.0 °C,
Time <=3600 sec
<= 0.20 %
@Temperature <=194 °F,
Time <=1.00 hour
parallel; IEC 60674-2
 <= 0.20 %
@Temperature <=90.0 °C,
Time <=3600 sec
<= 0.20 %
@Temperature <=194 °F,
Time <=1.00 hour
parallel; IEC 60674-2
 
Optical PropertiesMetricEnglishComments
Gloss 3.0 %3.0 %60°C top side; ASTM D2457
 7.0 %7.0 %60°C reverse side; ASTM D2457
Transmission, Visible >= 20 %>= 20 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrofol® BL 6-2 820803 Polycarbonate
Teijin Panlite® ML-1105 Light Diffusion Grade Polycarbonate
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® DE 1-1 000000 Polycarbonate

PB09865 / 92705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.