MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Angst+Pfister APSOplast® UP GM 203-1 UP GM Hm 2471
Categories: Polymer; Thermoset

Material Notes: (polyester resin glass filament mat)

General description: In cases where laminated paper is not strong enough but the top values of laminated glass fabric are not required, polyester resin laminated glass mat makes for an inexpensive alternative. This grade impresses users with its high mechanical strength and top electrical insulation. As well as complying with the most import ant standards, polyester resin laminated mats are suitable for further requirements. Due to the good electrical properties of this grade, it is used successfully in the electrical industry. Winding supports for dry transformers, partitions, switch levers in high-voltage switches, and insulators for choke coils – just some of the numerous poss ible uses.

Characteristics and properties:

  • High dimensional stability
  • Very good dielectric properties
  • High temperature resistance, temperature limit of +155 °C as per VDE (Heat Insulation Class F)
  • Self-extinguishing, meets the requirements of UL94 V-0 from 2.4 mm (type GPO-3)
  • High track and arc resistance (type GPO-3)

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.81 g/cc0.0654 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.0 MPa10200 psiISO 527
Modulus of Elasticity 9.00 GPa1310 ksiflexural test; ISO 178
Flexural Strength 130 MPa18900 psiISO 178
Compressive Strength 250 MPa36300 psiresistance, perpendicular to layers; ISO 604
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/3C
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 23.0 kV/mm584 kV/inat 90°C in oil parallel to layers; IEC 60243-1
Dielectric Loss Index 0.0100.010after 24 h immersed in water; DIN 53483
Comparative Tracking Index 600 V600 V[kV], at 90°C in oil parallel to layers; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.0 - 30.0 µm/m-°C11.1 - 16.7 µin/in-°FVDE 0304/2
Thermal Conductivity 0.274 W/m-K1.90 BTU-in/hr-ft²-°FDIN 52612
Flammability, UL94 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
 
Descriptive Properties
Colorwhite
Disruptive discharge voltage41

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP103 / 250601

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.