MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAPEX® ESC-70/AB Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: Sodium Laureth Sulfate

CAS: 68585-34-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAPEX ESC-70/AB is used in the formulation of high quality shampoos, bath products, liquid soaps and related cosmetic products. The viscosity of these sodium lauryl ethoxy sulfate based formulations can be adjusted by the addition of inorganic salts, Rhodamox OB/EBA, Mirataine BET C-30, and/or Alkamide DC-212/S. The mildness of a product formulated with RHODAPEX ESC-70/AB may be improved by the inclusion of cocoamphoacetates, like Miranol C2M-NP or high purity amphoterics like the Miranol Ultra.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
pH 7.0 - 9.07.0 - 9.04% Solution; RP-17601
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 90 %
@Wavelength 440 nm
>= 90 %
@Wavelength 440 nm
RP-17605
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceHazy, Viscous LiquidRP-17620
CompositionActive69-71%, MW 429, RP-17501
 Sodium Chloride<0.5%, MW 58.5, RP-17504
 Sodium Sulfate<2%, MW 142, RP-17503
 Unsulfate Matter<2.5%, RP 17303
OdorCharacteristic
Setting point6°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAPEX® ESB-70/A2 Surfactant
Solvay RHODAPEX® ES STD Surfactant
Solvay RHODAPEX® EAC-70 Surfactant
Solvay RHODAPEX® EA-2 Surfactant
Solvay RHODAPEX® EST-30/BLB Surfactant

WRHOD385 / 137616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.