MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SYNTHOS Krasten® 562E High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of plates, sheets, technical parts and molded packaging (used in e.g. the food and dairy industry).

Synthos was formerly known as Kaucuk. All information provided by Synthos.

Key Words: HIPS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inInternal; 50x50mm
Melt Flow 3.0 - 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 - 4.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Granulate; ISO 1133/H
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 65.0 MPa9430 psiFm=358N; Ø 50x4mm; ISO 2039-1
Tensile Strength at Break 25.0 MPa
@Temperature 23.0 °C
3630 psi
@Temperature 73.4 °F
50mm/min; ISO 527-2/1A/50
Tensile Strength, Yield 30.0 MPa
@Temperature 23.0 °C
4350 psi
@Temperature 73.4 °F
50mm/min; ISO 527-2/1A/50
Elongation at Break 45 %45 %50mm/min; ISO 527-2/1A/50
Tensile Modulus 2.00 GPa
@Temperature 23.0 °C
290 ksi
@Temperature 73.4 °F
1mm/min; ISO 527-2/1A/1
Flexural Strength 38.0 MPa
@Temperature 23.0 °C
5510 psi
@Temperature 73.4 °F
2mm/min; 80x10x4mm; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 180/1A
Izod Impact, Unnotched (ISO) 100 kJ/m²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 180/1U
Charpy Impact Unnotched  13.0 J/cm²
@Temperature 23.0 °C
61.9 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
80x10x4mm; ISO 179/1fU
Charpy Impact, Notched 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
80x10x4mm, r=0.25; V-notch; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cm500V; Ø 93x3mm; IEC 93
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm500V; Ø 93x3mm; IEC 93
Dielectric Constant <= 3.0
@Frequency 50 Hz
<= 3.0
@Frequency 50 Hz
500V; Ø 93x3mm; IEC 250
Dielectric Strength >= 28.0 kV/mm>= 711 kV/inTransformer Oil; Ø 93x3mm; IEC 243-1
Dissipation Factor <= 0.0010
@Frequency 50 Hz
<= 0.0010
@Frequency 50 Hz
500V; Ø 93x3mm; IEC 250
Arc Resistance >= 70 sec>= 70 secØ 93x3mm; IEC 61 621
Comparative Tracking Index >= 300 V>= 300 VSolution A; Ø 93x3mm; IEC 112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °F80x10x4mm; ISO 75-2/Af
Vicat Softening Point 88.0 °C190 °F50°C/h; 50N; 10x10x4mm; ISO 306/B50
 94.0 °C201 °F120°C/h; 50N; 10x10x4mm; ISO 306/B120
 98.0 °C208 °F50°C/h; 10N; 10x10x4mm; ISO 306/A50
 100 °C212 °F120°C/h; 10N; 10x10x4mm; ISO 306/A120
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Tested in EZÚ Praha
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Tested in EZÚ Praha
Glow Wire Test 650 °C1200 °FØ 93x3mm; IEC 695-2-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow AIM® 4900 High Impact Styrenic Resin
Ineos Nova 2114 High Impact Polystyrene Extrusion Grade
Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene
NIZHNEKAMSKNEFTEKHIM 825E High Impact Polystyrene
NIZHNEKAMSKNEFTEKHIM 825ES High Impact Polystyrene

PSYNT014 / 82627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.