MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ChevronTexaco Vistac® ISO 68 Way Oil D
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Way Oils Vistac D are high quality lubricants designed to meet the critical lubrication demands for the slides and ways of machine tools.

Chevron Way Oils Vistac D is formulated with high quality base stocks and an additive system that provides extreme pressure and antiwear protection, foam suppression, thermal stability, and demulsification.

As indicated by the name, Vistac, these lubricants provide an unusual adhesive or tacky quality. Chevron Way Oils Vistac D reduce leakage and adhere to metal surfaces providing a tenacious lubricant film. Due to their adhesiveness, these oils form a tenacious film which resists being wiped away by the slowly moving parallel surfaces of the way or being washed away by cutting fluids.

Chevron Way Oils Vistac D are friction modified to meet the exacting lubrication demands for the slides and ways of machine tools. Their inherent low coefficient of static friction eliminates "stick-slip" or jerky motion of sliding parts on machine tools, which increase operating efficiency of the tools and smoother overall operation.

Chevron Way Oils Vistac D provide excellent way oil separation from the metalworking coolant in the reservoir, reducing the adverse affect of tramp oil on the coolant stability.

Their antiwear and extreme pressure properties protect the sliding surfaces.

These oils protect cast iron and bronze surfaces from rust and corrosion, and are resistant to oxidation to provide long lubricant life.

Applications

Chevron Way Oils Vistac D have proven excellence in the lubrication of ways in many types of machine tools, e.g. lathes, planers, shapers, drilling and tapping machines, etc., including those operating at high loads. Chevron Way Oils Vistac D have been successfully field tested in Okuma and Moriseiki machine tools.

These oils perform well in the lubrication of enclosed gears and all types of industrial plain and antifriction bearings. Additionally, their tacky quality makes these oils suitable for once-through applications, e.g. lubrication of chain drives.

Chevron Way Oils Vistac D meet the requirements of:

  • Cincinnati Machine under their P-53 (ISO 32), P-47 (ISO 68), and P-50 (ISO 220) specifications for way lubricants.
  • General Motors LS2 Specification LW for way lubricants (ISO 68, 220).
Chevron Way Oils Vistac D pass the Bijur filterability test.

Key Words: CPS Number: 232516; MSDS Number: 7993
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 31 °31 °
Viscosity Measurement 104104Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 334 SUS334 SUS
Saybolt Viscosity at 210°F 55.2 SUS55.2 SUS
Kinematic Viscosity at 40°C (104°F) 64.6 cSt64.6 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 8.6 cSt8.6 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -18.0 °C-0.400 °FASTM D97
Flash Point 250 °C482 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCHEV383 / 74998

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.