MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

ITW Chockfast® Red HF Epoxy Grouting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: CHOCKFAST® Red HF Epoxy Grout is a three-component, epoxy-based grouting compound designed to improve the installation of grout in difficult machinery and equipment installations. CHOCKFAST® Red HF Epoxy Grout is ideal for establishing the long-term support and alignment required by the most demanding industrial machinery installations and operational conditions. CHOCKFAST® Red HF Epoxy Grout is available in red or a neutral white color.

USE & BENEFITS CHOCKFAST® Red HF Epoxy Grout offers improved working and placement qualities. It is suitable for small and large volume pours - achieving excellent cured properties for dependable, long-term service.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.05 g/cc0.0740 lb/in³ASTM C905
Brookfield Viscosity  2500 - 7500 cP
@Temperature 32.2 °C
2500 - 7500 cP
@Temperature 90.0 °F
mixed, A&B only. Brookfield viscosity/HBT 20rpm.
 6000 - 16000 cP
@Temperature 21.1 °C
6000 - 16000 cP
@Temperature 70.0 °F
mixed, A&B only. Brookfield viscosity/HBT 20rpm.
 25000 - 37000 cP
@Temperature 32.2 °C
25000 - 37000 cP
@Temperature 90.0 °F
mixed, A,B &C. Brookfield viscosity/HBT 20rpm.
 35000 - 55000 cP
@Temperature 21.1 °C
35000 - 55000 cP
@Temperature 70.0 °F
mixed, A,B &C. Brookfield viscosity/HBT 20rpm.
 >= 60000 cP
@Temperature 10.0 °C
>= 60000 cP
@Temperature 50.0 °F
mixed, A,B &C. Brookfield viscosity/HBT 20rpm.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 20.0 MPa2900 psiASTM D638
Flexural Strength 35.9 MPa5200 psiASTM C580
Flexural Modulus 10.7 GPa1550 ksiASTM C580
Compressive Strength 95.8 MPa13900 psiASTM C579 MOD
Compressive Modulus 1.10 GPa160 ksiASTM C579 MOD
Adhesive Bond Strength 10.7 MPa1550 psiConcrete; ASTM C882
 14.1 MPa2050 psiSteel; ASTM C-1002
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.4 µm/m-°C19.1 µin/in-°FASTM C531
Shrinkage 0.00 %0.00 %Negligible; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  1440 min
@Pressure 4.27 MPa,
Temperature 10.0 °C
24.0 hour
@Pressure 620 psi,
Temperature 50.0 °F
Ambient
 1440 min
@Pressure 21.4 MPa,
Temperature 21.1 °C
24.0 hour
@Pressure 3100 psi,
Temperature 70.0 °F
Ambient
 1440 min
@Pressure 77.9 MPa,
Temperature 32.2 °C
24.0 hour
@Pressure 11300 psi,
Temperature 90.0 °F
Ambient
 4320 min
@Pressure 24.1 MPa,
Temperature 10.0 °C
72.0 hour
@Pressure 3500 psi,
Temperature 50.0 °F
Ambient
 4320 min
@Pressure 77.2 MPa,
Temperature 21.1 °C
72.0 hour
@Pressure 11200 psi,
Temperature 70.0 °F
Ambient
 4320 min
@Pressure 87.6 MPa,
Temperature 32.2 °C
72.0 hour
@Pressure 12700 psi,
Temperature 90.0 °F
Ambient
 10100 min
@Pressure 62.1 MPa,
Temperature 10.0 °C
168 hour
@Pressure 9000 psi,
Temperature 50.0 °F
Ambient
 10100 min
@Pressure 89.6 MPa,
Temperature 21.1 °C
168 hour
@Pressure 13000 psi,
Temperature 70.0 °F
Ambient
 10100 min
@Pressure 94.5 MPa,
Temperature 32.2 °C
168 hour
@Pressure 13700 psi,
Temperature 90.0 °F
Ambient
Working Life  90.0 min
@Temperature 32.2 °C
90.0 min
@Temperature 90.0 °F
 150 min
@Temperature 21.1 °C
150 min
@Temperature 70.0 °F
 >= 240 min
@Temperature 10.0 °C
>= 240 min
@Temperature 50.0 °F
Shelf Life 12.0 Month12.0 MonthIn dry storage
 
Descriptive Properties
Effective Bearing Area> 95%ASTM C1339
Fire Resistanceself extinguishingASTM D635
Peak Exothermic Temp. (°F)130 to 150@ 70°F
 150 to 160@ 90°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWC9022 / 239532

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.