MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also be used under high working temperatures.

Information provided by Hippe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccDIN 53 479
Moisture Absorption at Equilibrium 1.5 %Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 5.5 %DIN 53 495
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 200 - 270 MPa
@Time 30.0 sec
DIN 53 456
Elongation at Break 3.5 %dry; DIN 53 455
 5.0 %cond.; DIN 53 455
Tensile Modulus 7.50 GPacond.; DIN 53 457
 9.70 GPadry; DIN 53 457
Charpy Impact, Notched 13.0 - 17.0 kJ/m²DIN 53 453
Coefficient of Friction, Dynamic 0.45 - 0.50Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 140in MPa; Cond.; DIN 53 455
 200in MPa; dry; DIN 53 455
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 30.0 µm/m-°C
Specific Heat Capacity 1.50 J/g-°C
Thermal Conductivity 0.270 W/m-K
Melting Point 255 °CDIN 53 736
Maximum Service Temperature, Air 110 °CContinuous use
 200 °CShort Periods
Deflection Temperature at 0.46 MPa (66 psi) 250 °CISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO-R 75 Method A
Glass Transition Temp, Tg 5.00 °Ccond., dynamic; DIN 53 736
 50.0 °Cdry, dynamic; DIN 53 736
Flammability, UL94 HB
 
Descriptive Properties
Colorblack
Creep ResistanceGrade CTI 475DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, sudsresistant in some conditions

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EPICHEM PA 66 GF 30 Polyamide 66, 30% Glass
Overview of materials for Nylon 66, 30% Glass Fiber Filled
Covestro Texin® 970 U Thermoplastic Polyurethanes (TPU)
Envalior Akulon® S223-D PA66, Dry
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester

PHIPPE973 / 121977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.