MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoset Polyester Glass SMC
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyester Glass SMC". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.810 - 2.01 g/ccAverage value: 1.77 g/cc Grade Count:203
Filler Content 18.0 - 40.0 %Average value: 25.9 % Grade Count:32
Water Absorption 0.000 - 1.10 %Average value: 0.294 % Grade Count:163
 1.20 - 1.20 %
@Temperature 50.0 - 50.0 °C
Average value: 1.20 % Grade Count:1
 1.20 - 1.20 %
@Time 3.60e+6 - 3.60e+6 sec
Average value: 1.20 % Grade Count:1
Linear Mold Shrinkage -0.00100 - 0.0200 cm/cmAverage value: 0.00107 cm/cm Grade Count:149
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 15.0 - 74.0Average value: 49.5 Grade Count:73
Hardness, Rockwell M 70.0 - 116Average value: 87.0 Grade Count:25
Tensile Strength, Ultimate 13.0 - 2590 MPaAverage value: 101 MPa Grade Count:174
 64.0 - 64.0 MPa
@Temperature 150 - 150 °C
Average value: 64.0 MPa Grade Count:1
Tensile Strength, Yield 13.0 - 160 MPaAverage value: 72.7 MPa Grade Count:33
Elongation at Break 0.000 - 1.80 %Average value: 0.570 % Grade Count:43
Modulus of Elasticity 2.76 - 88.2 GPaAverage value: 12.5 GPa Grade Count:116
 9.30 - 9.30 GPa
@Temperature 150 - 150 °C
Average value: 9.30 GPa Grade Count:1
Flexural Yield Strength 50.0 - 1000 MPaAverage value: 179 MPa Grade Count:208
 108 - 557.096 MPa
@Temperature 120 - 160 °C
Average value: 269 MPa Grade Count:2
 65.0 - 65.0 MPa
@Temperature 130 - 130 °C
Average value: 269 MPa Grade Count:1
 65.0 - 65.0 MPa
@Thickness >=1.50 mm
Average value: 269 MPa Grade Count:1
Flexural Modulus 3.00 - 55.2 GPaAverage value: 10.6 GPa Grade Count:189
 8.00 - 27.0 GPa
@Temperature 120 - 160 °C
Average value: 20.3 GPa Grade Count:2
Compressive Yield Strength 74.5 - 379 MPaAverage value: 180 MPa Grade Count:95
Compressive Modulus 6.89 - 17.2 GPaAverage value: 10.3 GPa Grade Count:8
Ultimate Bearing Strength 221 MPaAverage value: 221 MPa Grade Count:6
Poissons Ratio 0.300Average value: 0.300 Grade Count:66
Shear Modulus 1.30 - 5.80 GPaAverage value: 4.09 GPa Grade Count:66
Shear Strength 31.0 - 124 MPaAverage value: 67.7 MPa Grade Count:23
 33.7843 - 39.9896 MPa
@Temperature 120 - 160 °C
Average value: 36.9 MPa Grade Count:1
Izod Impact, Notched 0.640 - 26.7 J/cmAverage value: 7.65 J/cm Grade Count:129
Izod Impact, Unnotched 3.20 - 15.0 J/cmAverage value: 9.08 J/cm Grade Count:54
Charpy Impact Unnotched 5.00 - 60.0 J/cm²Average value: 9.71 J/cm² Grade Count:23
Charpy Impact, Notched 1.90 - 17.0 J/cm²Average value: 7.05 J/cm² Grade Count:42
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 - 1.00e+16 ohm-cmAverage value: 1.04e+15 ohm-cm Grade Count:44
Surface Resistance 1e+05 - 1.00e+14 ohmAverage value: 3.21e+13 ohm Grade Count:54
Dielectric Constant 4.00 - 5.20Average value: 4.31 Grade Count:54
Dielectric Strength 1.38 - 47.2 kV/mmAverage value: 16.8 kV/mm Grade Count:113
 1.85039 - 23.0 kV/mm
@Temperature 90.0 - 90.0 °C
Average value: 10.9 kV/mm Grade Count:2
 2.3622 - 10.0 kV/mm
@Temperature 90.0 - 90.0 °C
Average value: 10.9 kV/mm Grade Count:1
 2.3622 - 10.0 kV/mm
@Thickness 3.00 - 3.00 mm
Average value: 10.9 kV/mm Grade Count:1
Dielectric Breakdown 54000 - 60000 VAverage value: 56000 V Grade Count:4
Dissipation Factor 0.00300 - 0.0600Average value: 0.0152 Grade Count:48
Arc Resistance 100 - 194 secAverage value: 169 sec Grade Count:77
Comparative Tracking Index 500 - 601 VAverage value: 593 V Grade Count:67
 
Thermal PropertiesOriginal ValueComments
CTE, linear -1.02 - 36.0 µm/m-°CAverage value: 21.2 µm/m-°C Grade Count:82
CTE, linear, Transverse to Flow 20.0 - 27.0 µm/m-°CAverage value: 25.0 µm/m-°C Grade Count:33
Specific Heat Capacity 1.10 - 1.51 J/g-°CAverage value: 1.13 J/g-°C Grade Count:38
Thermal Conductivity 0.250 - 0.700 W/m-KAverage value: 0.486 W/m-K Grade Count:73
Maximum Service Temperature, Air 130 - 300 °CAverage value: 176 °C Grade Count:65
Maximum Service Temperature, Inert 130 - 180 °CAverage value: 157 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 150 - 260 °CAverage value: 213 °C Grade Count:102
Minimum Service Temperature, Air -40.0 °CAverage value: -40.0 °C Grade Count:33
Glass Transition Temp, Tg 125 - 210 °CAverage value: 171 °C Grade Count:34
UL RTI, Electrical 120 - 160 °CAverage value: 131 °C Grade Count:28
UL RTI, Mechanical with Impact 130 - 150 °CAverage value: 131 °C Grade Count:26
UL RTI, Mechanical without Impact 130 - 160 °CAverage value: 132 °C Grade Count:27
Flammability, UL94 HB - 5VAGrade Count:115
Flame Spread Index 12.9 - 25.0Average value: 20.1 Grade Count:8
Smoke Density 600 - 700Average value: 650 Grade Count:3
Oxygen Index 20.0 - 70.0 %Average value: 26.4 % Grade Count:33
Glow Wire Test 690 - 960 °CAverage value: 830 °C Grade Count:41
 
Processing PropertiesOriginal ValueComments
Processing Temperature 120 - 160 °CAverage value: 147 °C Grade Count:69
Mold Temperature 140 - 160 °CAverage value: 150 °C Grade Count:23
Cure Time 120 - 120 min
@Temperature 200 - 200 °C
Average value: 188 min Grade Count:1
 960 - 960 min
@Temperature 80.0 - 80.0 °C
Average value: 188 min Grade Count:1
 960 - 960 min
@Pressure 0.621 - 0.621 MPa
Average value: 188 min Grade Count:1
 1.25 - 5.00 min
@Temperature 138 - 149 °C
Average value: 188 min Grade Count:4
 1.25 - 5.00 min
@Thickness 1.52 - 6.35 mm
Average value: 188 min Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass Filled BMC
Applied Composites 120 Polyester SMC
Overview of materials for Polyester (Thermoset) - Rigid
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Polyester Thermoplastic Elastomer, Glass Filled

O3510 / 78219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.