A 302 HF is light blue putty formulated from unsaturated polyester resins and glass fibers that gel and cure at room temperature by adding MEKP catalyst. This material may be used to bond different substrates. It is excellent putty for sanitary, transportation, nautical and general purpose applications. Features And Benefits: - A 302 HF is easily applied by using an appropriate tool such as spatula or a trowel.
- Formulated to use with MEKP catalyst.
- Excellent adhesion of fiberglass to fiberglass and wood to fiberglass.
- Fast gel time and excellent cure
- Color indicator to ensure proper catalyst mix.
Information provided by Polynt Composites. |