System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Americhem Engineered Compounds ColorFast® NYA1000 Nylon/ABS Alloy
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
;
Nylon (Polyamide PA)
Material Notes:
Nylon/ABS alloy with high ductility and excellent chemical resistance
All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.
Key Words:
Nylon, ABS
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.08
g/cc
ASTM D792
Linear Mold Shrinkage
0.0070
in/in
0.125 in.; ASTM D955
Melt Flow
9.0
g/10 min
@Load 3.80 kg,
Temperature 260 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
6000
psi
2.0 in/min; ASTM D638
Elongation at Break
200 %
2.0 in/min; ASTM D638
Flexural Strength
8600
psi
2.0 in/min; ASTM D790
Flexural Modulus
170000
psi
2.0 in/min; ASTM D790
Izod Impact, Notched
12.0
ft-lb/in
@Temperature 22.8 °C
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
150
°F
Unannealed (0.250"); ASTM D648
Processing Properties
Original Value
Comments
Rear Barrel Temperature
400
-
460
°F
Middle Barrel Temperature
410
-
450
°F
Front Barrel Temperature
430
-
490
°F
Nozzle Temperature
420
-
480
°F
Melt Temperature
430
-
490
°F
Mold Temperature
50.0
-
160
°F
Drying Temperature
185
°F
Dry Time
3
-
4
hour
nominal; maximum drying time of 8 hours
Back Pressure
50.0
-
100
psi
Shot Size
40 - 60 %
Vent Depth
0.00100
-
0.00300
in
Screw Speed
40
-
70
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Daicel CEVIAN® A1700 PA/ABS Alloy, DAM
Techmer ES Plastiblend® ABS/PA 1700
E-Polymers TEKAMID® H12TW Unreinforced Low warpage PA/ABS Alloy
Polykemi AB SCANLON A 5005B PA/ABS-Blend
INEOS Styrolution Terblend® N NM-13 ABS/PA6 (Dry)
PLTLC045 / 104430
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.