MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos Styrenics 158K High-Heat Polystyrene Crystal Resin (Global)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Description: High-heat, high-molecular weight grades for a variety of applications, including medical devices and labware, cosmetics packaging, CD & DVD jewel boxes, food serviceware, and low-taste, low-odor products such as cook and cake trays as well as other oriented polystyrene (OPS) applications.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7676ASTM D785
Tensile Strength at Break 49.0 MPa7110 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 2.52 GPa366 ksiASTM D638
Flexural Modulus 3.24 GPa470 ksiASTM D790-1
Izod Impact, Notched 0.160 J/cm0.300 ft-lb/inASTM D256-A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °FASTM D648
Vicat Softening Point 109 °C228 °FASTM D1525
Flammability, UL94 HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
All Colors
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °FExtrusion
 180 - 280 °C356 - 536 °FMolding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ASA/PC FA-30
Trinseo EMERGE™ 4800-7 Polycarbonate
Trinseo EMERGE™ 7560 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Trinseo EMERGE™ 4800-10 Polycarbonate
Biomer P304 PHB Biodegradable Polymer

PSG100 / 67261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.