MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Pluracol® SG-450 Rigid Polyol
Categories: Fluid

Material Notes: Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent compatibility with blowing agents and isocyanates for appliance, high density and general purpose foam formulations. This polyol when combined with suitable flame retardants, yields foams having low smoke and good char-forming characteristics in the ASTM E-84 tunnel test*

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/cc
@Temperature 60.0 °C
 1.12 g/cc
@Temperature 40.0 °C
 1.15 g/cc
@Temperature 25.0 °C
Viscosity 2600 cP
@Temperature 60.0 °C
 10000 cP
@Temperature 40.0 °C
 35000 cP
@Temperature 25.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.050 %STI 3062
 
Descriptive Properties
ColorLight Colored Liquid
Hydroxyl Number440 - 460 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ethylene Urea
AISI 1095 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Sandvik Osprey SCM415 Low Alloy Steel Powder
NYC YT3WBHQ Y2O3 Powder for Spray Coating

PBASG0814 / 132447

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.