MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Kolon KOPA® KN3322V0 Nylon 66 (PA66), Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: PA66, Flame Retardant.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Water Absorption 0.90 %
@Time 86400 sec
0.90 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage 0.012 - 0.017 cm/cm0.012 - 0.017 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 80.0 MPa
@Thickness 3.20 mm
11600 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 15 %
@Thickness 3.20 mm
15 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 132 MPa
@Thickness 3.20 mm
19100 psi
@Thickness 0.126 in
5 mm/min; ASTM D790
Flexural Modulus 3.20 GPa
@Thickness 3.20 mm
464 ksi
@Thickness 0.126 in
5 mm/min; ASTM D790
Izod Impact, Notched 0.500 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
0.937 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F20°C/min; ASTM D1525
Deflection Temperature at 1.8 MPa (264 psi) 105 °C221 °FASTM D648
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 270 °C482 - 518 °F
Middle Barrel Temperature 250 - 270 °C482 - 518 °F
Front Barrel Temperature 255 - 275 °C491 - 527 °F
Nozzle Temperature 260 - 275 °C500 - 527 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 80.0 - 90.0 °C
@Time 10800 - 18000 sec
176 - 194 °F
@Time 3.00 - 5.00 hour
Dehumidifying Dryer
Moisture Content <= 0.10 %<= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ732 / 255743

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.