MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Rigid Extrusion 8700A Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes:

Note: Automotive OEM approval(s). Note: NSF listings are obtained on specific colors. The Cell Classification was determined using the notched Izod test with injection molded samples.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Hardness, Shore D 7815 sec; ASTM D2240
Tensile Strength, Yield 42.7 MPaType I, 5.1 mm/min; ASTM D638
Tensile Modulus 2690 MPaType I, 5.1 mm/min; ASTM D638
Flexural Strength 75.8 MPaASTM D790
Flexural Modulus 2620 MPaASTM D790
Compressive Strength 55.8 MPaASTM D695
Izod Impact, Notched 59.0 J/m
@Thickness 3.18 mm,
Temperature -18.0 °C
Compression Molded; ASTM D256A
 85.0 J/m
@Thickness 3.18 mm,
Temperature 0.000 °C
Compression Molded; ASTM D256A
 910 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Compression Molded; ASTM D256A
Dart Drop Total Energy 35.6 J/cm
@Temperature 23.0 °C
Procedure A, C.125; ASTM D4226
 35.6 J/cm
@Temperature 23.0 °C
Procedure B, C.125; ASTM D4226
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.3
@Frequency 1000 Hz
ASTM D150
 3.9
@Frequency 60 Hz
ASTM D150
Dielectric Strength 27.0 kV/mmASTM D149
Dissipation Factor 0.029
@Frequency 60 Hz,
Temperature 30.0 °C
24 hr; ASTM D150
 0.040
@Frequency 1000 Hz,
Temperature 30.0 °C
24 hr; ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 0.711 mm
ALL; UL 94
 V-0
@Thickness 0.870 mm
All Colors
 5VA
@Thickness 1.50 mm
ALL; UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 179 - 182 °C
 
Descriptive Properties
Agency RatingsNSF 51
 NSF 61
Automotive SpecificationsCHRYSLER MS-DC28 Type B CPN2647 Color: Black
 GM GM7001M (PVC)
Ease of SizingExcellent
FeaturesGeneral Purpose
 Good Dimensional Stability
 Good Melt Strength
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Processing MethodExtrusion
PVC Cell Classification16344ASTM D1784
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Beltline Moldings
 General Purpose
 Profiles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Extrusion 87345 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 80510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions 83510 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion 87775 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Extrusion L0678 Natural Polyvinyl Chloride, Rigid

PH0POL0016 / 144585

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.