MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ammonium Chloride, NH4Cl
Categories: Ceramic; Halide

Material Notes: CAS Number: 12125-02-9

Physical Form: Colorless Cubic Crystals

Key Words: NH4Cl
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.519 g/cc0.05488 lb/in³
Molecular Weight 53.492 g/mol53.492 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 1635.00 bar1.22635e+6 torr
Critical Temperature 882 °C1620 °F
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.572 J/g-°C0.3758 BTU/lb-°FCrystal
Boiling Point 338 °C640 °FSublimation Point
Heat of Formation -314.4 kJ/mol-314.4 kJ/molCrystal
Decomposition Temperature 5200 °C9390 °FTriple Point (decomposes)
 
Descriptive Properties
SolubilitySoluble in H2O

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MV Labs NH400 NH4Cl Ammonium chloride
Overview of materials for Urea Formaldehyde, Molded, Cellulose Filled
Antimony (V) Chloride, Sb2Cl5
Antimony (III) Iodide, SbI3
Antimony (III) Fluoride, SbF3

EINOR2045 / 4185

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.