Sequel 1580-UV 598F ANTHRACITE thermoplastic polyolefin material exhibits significantly greater mar resistance than conventional TPOs. Sequel 1580-UV 598F ANTHRACITE polyolefin is typically used for automotive applications that demand low warpage and low CLTE, as well as excellent scratch and mar resistance. Applications: Automotive Parts, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |