PPS, linear, unreinforced, impact modified Properties: dimensionally stable, good chemical resistance, Good electrical properties, good aging behavior, good fire behavior, high continuous used temperature, High strength, High stiffness, semi-crystalline Information provided by BARLOG plastics GmbH. |