MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Inov Chem NCP-9B Polyurethane adhesive
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Overview: This product is a two-component polyurethane adhesive. Specially used for bonding the lawn to the ground foundation.

Characteristics: This product has low viscosity and good adhesion to the lawn and foundation. It is a low-VOC environmentally friendly product that meets the new national standard testing. It has excellent characteristics such as high temperature resistance, high bonding strength, long service life, green environmental protection, waterproof and light resistance. Completely solve the problem of adhesion failure caused by poor water resistance and poor aging resistance of traditional glues.

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hourOpening time
 240 min4.00 hourInitial setting time
 1440 min24.0 hour
 
Descriptive Properties
Appearancebrown liquid
Operation temperature5-35°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM194 / 312723

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.