MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay IGEPAL® CA 210 Surfactant
Categories: Fluid

Material Notes: Description: Octyl phenol ethoxylate (1.5EO). Effective emulsifier for nonpolar solvents in solvent emulsion cleaners, pesticides, dry cleaning detergents and floor polishes. Nonionic dispersant and emulsifier for cosmetic formulations.

Chemical Name: OCTYLPHENOXY POLY(ETHYLENEOXY)ETHANOL, BRANCHED)

CAS: 9002-93-1; 7732-18-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: IGEPAL© CA-210 is a primary nonionic surfactant recommended especially for the emulsion polymerization of acrylic, vinyl acrylic, styrene butadiene and styrene acrylic polymers. Such polymers find application in latex paints, adhesives, paper coatings and textile applications. IGEPAL© CA-210 is one of a series of Rhodia ethoxylated alkylphenol nonionic surfactants with different HLBs. Since differences in HLB affect emulsification and stabilization properties, the Igepal series allows the user to select the surfactant that will provide effective particle size control, low levels of coagulum, latex stability and trouble-free commercial production.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cc
Viscosity 500 - 800 cP
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 4.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to Slightly Hazy LiquidRP-0064
HLB number4.8
Hydroxyl Number210-225 mg KOH/gRP-0245
Ionic ChargeNonionic
Neutralization Number<0.5 mg KOH/gpH7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay IGEPAL® CO 630 Surfactant

WRHOD144 / 137375

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.