MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow Agility™ 1001 Performance LDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Product Description: Agility 1001 Performance LDPE is a high pressure LDPE resin designed specifically to run at faster output rates on blown film lines in blends with LLDPE resins while maintaining bubble stability.
Main Characteristics:
  • Faster processing LDPE resin
  • Designed for higher output rates in blends with LLDPE resins at 10-20% loading
  • Optimized molecular structure gives improved optics in blends with LLDPE resins
Complies with: US FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection. Consult the regulations for complete details.

Availability: Europe; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520 ©2.2; EU No 10/2011; Canadian HPFB No Objection

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ASTM D792
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance 31.1 N7.00 lb (f)
Film Tensile Strength at Yield, MD 27.6 MPa4000 psiASTM D882
Film Tensile Strength at Yield, TD 12.8 MPa1850 psiASTM D882
Film Elongation at Break, MD 120 %120 %ASTM D882
Film Elongation at Break, TD 440 %440 %ASTM D882
1% Secant Modulus 236 MPa34200 psiMD; ASTM D882
 297 MPa43100 psiTD; ASTM D882
2% Secant Modulus 0.216 GPa31.4 ksiMD; ASTM D882
 0.256 GPa37.2 ksiTD; ASTM D882
Puncture Energy 1.02 J0.750 ft-lb
Elmendorf Tear Strength MD 270 g270 gASTM D1922
Elmendorf Tear Strength TD 95 g95 gASTM D1922
Dart Drop Test 70.0 g0.154 lbASTM D1709A
Film Tensile Strength at Break, MD 28.6 MPa4150 psiASTM D882
Film Tensile Strength at Break, TD 16.9 MPa2450 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 109 °C228 °F
Vicat Softening Point 93.9 °C201 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 9.0 %9.0 %ASTM D1003
Gloss 54 %54 %45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 203 °C398 °FExtrusion
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
Film Puncture Resistance60 ft-lb/in3
Film Toughness320 ft-lb/in3MD, ASTM D882
 650 ft-lb/in3TD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDOWF384 / 311077

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.