MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ketron® 1000 PEEK SP Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Ketron® 1000 PEEK SP stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron® PEEK SP grades. Both Ketron® 1000 PEEK SP natural & black can be sterilized by all conventional sterilization methods (steam, dry heat, ethylene oxide and gamma irradiation).

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccISO 1183-1
Water Absorption <= 0.060 %
@Time 86400 sec
ISO 62
Water Absorption at Saturation 0.45 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 105ISO 2039-2
Tensile Strength 115 MPaISO 527-1/-2
Elongation at Break 10 %ISO 527-1/-2
Elongation at Yield 4.0 %ISO 527-1/-2
Modulus of Elasticity 4.40 GPaISO 527-1/-2
Compressive Strength 40.0 MPa
@Strain 1 %
ISO 604
 80.0 MPa
@Strain 2 %
ISO 604
 140 MPa
@Strain 5.0 %
ISO 604
Charpy Impact Unnotched 390 kJ/m²ISO 179-1/1eU
Charpy Impact, Notched 2.80 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 62631-3-1
Surface Resistivity per Square 1.00e+13 ohmANSI/ESD STM 11.11
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 610 V/milIEC 60243-1
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
IEC 62631-2-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 100 °C
ASTM D696
 55.0 µm/m-°C
@Temperature 23.0 - 150 °C
ASTM D696
 130 µm/m-°C
@Temperature >=150 °C
ASTM D696
Thermal Conductivity 0.250 W/m-K
Melting Point 340 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-1/-2
Minimum Service Temperature, Air -50.0 °C
Flammability, UL94 V-0
@Thickness 3.00 mm
 
Descriptive Properties
Colorbrownish grey, black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM935 / 291092

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.