MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Huber Onyx Elite® 255 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Onyx Elite® 255 is a high purity alumina trihydrate used in the manufacture of solid surface cast polymers. Improved physical performance of solid surface materials results from the selected particle size distribution of Onyx Elite® 255. This product yields low viscosities, excellent air release, reduced matrix settling and a very homogenous casting. Onyx Elite® 255 has a broad particle distribution with a controlled top size (<5% on 100 mesh) which yields excellent packing characteristics. The median particle diameter, controlled particle distribution and low contaminant level of Onyx Elite® 255 aid manufacturers in obtaining good cure, good translucency and excellent color, when compared to other products offered for solid surface applications.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.42 g/cc2.42 g/cc
Bulk Density 1.00 g/cc0.0361 lb/in³loose
 1.50 g/cc0.0542 lb/in³packed
Moisture Absorption 0.100 %
@Temperature 105 °C
0.100 %
@Temperature 221 °F
Free
Particle Size <= 10 µm<= 10 µm37 percent
 30 µm30 µmMedian Particle Diameter
Particle Mesh Size 100 Mesh100 Mesh<5% on
 200 Mesh200 Mesh15-20% on
 325 Mesh325 Mesh50% on
 325 Mesh325 Mesh60% through
Specific Surface Area 1.5 m²/g1.5 m²/gBET
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.0040 %0.0040 %
Loss on Ignition(%) 34.5 %
@Temperature 1000 °C
34.5 %
@Temperature 1830 °F
Na2O 0.020 %0.020 %soluble
 0.20 %0.20 %total
SiO2 0.0080 %0.0080 %
 
Descriptive Properties
Al(OH)3 (%)99.6
Color89 L
FunctionalityLow Viscosity Aid
Functionality: Optical effectsHigh Brightness / Transparency
Market/Application: ThermosetsSolid Surface/Cast Polymer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER760 / 300866

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.