This alloy offer a good combination of flow and ductility. Like Matti-phos 6 it is used in air conditioning, refrigeration, medical gas pipework and heat exchanger manufacture. Optimum Joint Gap 0.05 - 0.2 mm. AWS A5.8-92 BCuP-3 BS EN 1044 1999 CP104 Federal Specification QQ-B-650 BcuP-1 Equivalent to Engelhard Silvaloy 5 Equivalent to Handy & Harman Sil Fos 5 Equivalent to J W Harris Stay-Silv 5 Information provided by Johnson Matthey. |