MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polymer Resources NY6-G13-[color]-H Nylon 6, 13% Glass Reinforced, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Nylon 6, 13% Glass Reinforced, Heat Stabilized, Lubricated

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).

Information provided by Polymer Resources Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 19000 psiASTM D638
Tensile Strength, Yield 19000 psiASTM D638
Flexural Strength 26000 psiASTM D790
Flexural Modulus 800 ksiASTM D790
Izod Impact, Notched 1.10 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 390 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
 HB
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 480 - 515 °F
Middle Barrel Temperature 470 - 500 °F
Front Barrel Temperature 480 - 515 °F
Melt Temperature 480 - 515 °F
Mold Temperature 150 - 220 °F
Drying Temperature 165 - 185 °F
Dry Time 3.00 - 4.00 hour
Vent Depth 0.000500 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned)
Ashley Polymers Ashlene® 830L-13G Nylon 6, 13% Glass Reinforced
Ashley Polymers Ashlene® 630-13G Nylon 6, 13% Glass Reinforced
Asahi Kasei Thermofil N-13FG-1626 13% Glass Fiber Reinforced, Heat Stabilized Nylon 6

PPOLYQ062 / 160578

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.