MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sandvik 19.12.3.LSi Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 19.12.3.Nb is a niobium stabilized filler metal suitable for joining stainless steels of the 18Cr/8Ni/Mo, 18Cr/8Ni/Mo/Ti and 18Cr/8Ni/Mo/Nb types. Due to the strengthening effect of niobium, this grade is recommended if the weld metal will be exposed to temperatures above 400°C (750 F).

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160160
Tensile Strength, Ultimate  440 MPa
@Temperature 400 °C
63800 psi
@Temperature 752 °F
 610 MPa
@Temperature 20.0 °C
88500 psi
@Temperature 68.0 °F
Tensile Strength, Yield  290 MPa
@Strain 0.2 %,
Temperature 400 °C
42100 psi
@Strain 0.2 %,
Temperature 752 °F
 400 MPa
@Strain 0.2 %,
Temperature 20.0 °C
58000 psi
@Strain 0.2 %,
Temperature 68.0 °F
Elongation at Break  29 %
@Temperature 400 °C
29 %
@Temperature 752 °F
 37 %
@Temperature 20.0 °C
37 %
@Temperature 68.0 °F
Reduction of Area 68 %68 %
Charpy Impact  50.0 J
@Temperature -196 °C
36.9 ft-lb
@Temperature -321 °F
 130 J
@Temperature 20.0 °C
95.9 ft-lb
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  15.0 W/m-K
@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 16.0 W/m-K
@Temperature 100 °C
111 BTU-in/hr-ft²-°F
@Temperature 212 °F
 19.0 W/m-K
@Temperature 300 °C
132 BTU-in/hr-ft²-°F
@Temperature 572 °F
 21.0 W/m-K
@Temperature 500 °C
146 BTU-in/hr-ft²-°F
@Temperature 932 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.020 %0.020 %All Weld Metal
 <= 0.025 %<= 0.025 %AIM
 <= 0.025 %<= 0.025 %Nominal
Chromium, Cr 18.3 %18.3 %Nominal
 18.5 %18.5 %All Weld Metal
 18.5 %18.5 %AIM
Manganese, Mn 1.7 %1.7 %All Weld Metal
 1.8 %1.8 %AIM
 1.8 %1.8 %Nominal
Molybdenum, Mo 2.6 %2.6 %AIM
 2.6 %2.6 %Nominal
 2.6 %2.6 %All Weld Metal
Nickel, Ni 11.5 %11.5 %All Weld Metal
 12 %12 %AIM
 12.3 %12.3 %Nominal
Nitrogen, N 0.050 %0.050 %Nominal
 0.060 %0.060 %All Weld Metal
 <= 0.060 %<= 0.060 %AIM
Phosphorus, P 0.010 %0.010 %All Weld Metal
 <= 0.025 %<= 0.025 %AIM
 <= 0.025 %<= 0.025 %Nominal
Silicon, Si 0.90 %0.90 %AIM
 0.90 %0.90 %Nominal
 0.90 %0.90 %All Weld Metal
Sulfur, S 0.013 %0.013 %All Weld Metal
 <= 0.015 %<= 0.015 %AIM
 <= 0.015 %<= 0.015 %Nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NSANDV5087 / 199651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.