MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot BLACK PEARLSĀ® 4040 Specialty carbon black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: BLACK PEARLS 4040 specialty carbon black is suitable for use in applications requiring a balance of ultraviolet (UV) protection, weatherability performance, and covering power particularly in film and sheet applications where surface smoothness is desired.

Key applications: BLACK PEARLS 4040 specialty carbon black can be used in a range of film and sheet applications including:

  • Mulch and silage film
  • Irrigation pipe and tape
  • General purpose film and sheet
Performance features: When exposed to sunlight and the associated ultraviolet (UV) rays, plastic film can degrade. BLACK PEARLS 4040 specialty carbon black can help protect plastic film, sheet, and pipe from UV degradation by absorbing UV rays. Its good covering power enables film & sheet applications to prevent sunlight transmission which is particularly important for applications such as agricultural film. In addition, its dispersion characteristics deliver good surface smoothness and low surface defects, helping to ensure high carbon black performance with respect to UV and covering power while preserving the mechanical integrity of the film. BLACK PEARLS 4040 specialty carbon black used in film and sheet applications can help extend the useful life of the final product due to its:
  • Good covering power, which prevents sunlight transmission in the film
  • Long-term UV and weatherability protection
  • Excellent surface smoothness and dispersion performance

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 325 Mesh<25 ppm; ASTM D-3265
 
Descriptive Properties
Iodine absorption82 mg/gASTM D-1510
OAN103 cc/100gASTM D-2414
Product FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT020 / 315755

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.