MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay RHODAPEX® AB 20 Surfactant
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: APE free ether sulfate surfactant for emulsion polymerization

Identification: AMMONIUM SALT OF SULPHATED ALCOHOL ETHOXYLATE.

CAS: 67762 – 19 – 0

Solubility: Soluble in water and most polar solvents. Insoluble in aromatic solvents.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Fabric and Home Care: Biodegradable anionic emulsifier, compatible with high levels of alcohol. Allows clear formulations. Industrial formulations: Anionic emulsifier. Polymer System Specialties: Emulsifier. Surfactant for emulsion polymerization. Most suited for acrylic and styrene/acrylic latex.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
pH 8.0 - 9.05% in water; RPG02
Surface Tension 40 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Pour Point 5.00 °C
Flash Point >= 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0RPG18
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceLimpid liquidRPG31
CompositionActive0.29
 Anionic substance on dry matter82-100, RPG12
 Dry substance28-29%, RPG25
Critical Micelle Concentration (%)0.03
Ionic ChargeAnionic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay RHODAPEX® CD-128 Surfactant
Solvay RHODAPEX® CO-436 Surfactant
Solvay RHODAPEX® EA-2 Surfactant
Solvay RHODAPEX® ES-2/K Surfactant
Solvay RHODAPEX® ESB-70/A2 Surfactant

WRHOD375 / 137606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.