Data provided by DuPont Packaging Polymers. SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile strength, puncture strength, elongation and heat seal strength compared to conventional films. Ideal for lamination to other substrates such as Dartek nylon film or Mylar polyester film for vacuum packaging applications. SL, in converter combinations, is particularly suited for the vacuum packaging of processed meats. |
Linear Low Density Polyethylene |