MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AGC FL1650 PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Product Description: Fluon® FL1650 is a finely milled PTFE (polytetrafluoroethylene). It is especially suitable for thermoplastic applications. This micropowder may also be used for compounding in rubber and thermoset products. The rounded particle shape and intermediate hardness permit mixing without further breakdown and without large increases in viscosity. This product is FDA compliant for food contact applications. FL1650 also features a low volatile content which may have value in specialized applications.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.440 g/cc0.0159 lb/in³ASTM D4894
Particle Size 13 µm13 µmD10, Low Shear
 17 µm17 µmHegman; ASTM D1210
 40 µm40 µmAverage, Low Shear
 95 µm95 µmD90, Low Shear
Specific Surface Area 1.0 m²/g1.0 m²/gKrypton
 
Thermal PropertiesMetricEnglishComments
Melting Point 335 °C635 °FASTM D3417
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM D4019
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AGC Fluon® PFA P62X White Pigmentation
AGC Fluon® PTFE
Beijing Evergrow Resources PTFE Bar
Celanese Celcon® MT8U01 Medical Grade Acetal Copolymer
Chemours Teflon® PTFE 7A Granular Molding Powder

PAGCX120 / 191229

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.