MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Clwyd Compounders AEM Acrylic Ethylene Copolymer
Categories: Polymer

Material Notes: AEM elastomers are primarily used where combined resistance to ozone, heat and oils is required. They are sometimes a good alternative to more expensive heat resistant elastomers such as fluorocarbon polymers (FKM), silicones (VMQ) and fluorosilicones (FVMQ) for elevated temperature applications (< 150 °C). However, AEMs are not recommended for exposure to aromatic hydrocarbons, gasoline, brake fluids and phosphate esters.

Typical applications: Typical applications include automotive transmission / power steering seals and O-rings that have to be resistant to transmission fluids and many other common automotive lubricants and hydraulic fluids. Other applications include diaphragms, plumbing seals, boots, hoses, vibration mounts, pads, isolators and custom molded rubber goods and parts.The typical continuous operating temperature range is -30°C to 150°C (up to 175°C for limited periods of time).

Advantages:

  • Excellent resistance to petroleum fuel and oil
  • Good heat resistance
  • Good ozone resistance
  • Resists flex cracking
Disadvantages:
  • Moderate water resistance

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 9045 - 90
Tensile Strength <= 20.0 MPa<= 2900 psi
Elongation at Break <= 350 %<= 350 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 175 °C347 °FUpper continuous
Minimum Service Temperature, Air -60.0 °C-76.0 °Fnon-brittle
 -40.0 °C-40.0 °Fsealing applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCLWYD014 / 316031

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.