MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

DIAB TBR® 8 Multifunctional Polymer Core Material  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Renewable/Recycled Polymer

Material Notes: TBR® is a multifunctional polymer core designed for hard points within sandwich structures where through-bolting or point-loading would normally cause local crushing of low density sandwich cores. TBR® provides strength and performance for applications where there is a need for hard points and through bolting while maintaining lightweight construction. Typical applications include bolt transoms (outboard and inboard/outboard), deck cleat and railing bases winch pads, strut bases, and thru-hull pads. TBR® is available in three densities as standard sheets or fabricated kits. TBR® may contain up to 10% recycled content. It has a highly imidized chemical structure within its inter-penetrating polymer network. TBR® has a coarse cell structure designed for increased mechanical adhesion.

Information provided by DIAB, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.128 g/cc0.00463 lb/in³Nominal
 0.115 - 0.154 g/cc0.00417 - 0.00556 lb/in³Tolerance from nominal of -10%/+20%; ASTM D1622
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 3.79 MPa550 psiASTM D1623
Elongation at Break 11.5 %11.5 %Shear Strain; ASTM C273
Compressive Strength 2.55 MPa370 psiASTM D1621
Compressive Modulus 0.172 GPa25.0 ksiASTM D1621-B
Poissons Ratio 0.320.32
Shear Modulus 0.0469 GPa6.80 ksiASTM C273
Shear Strength 1.90 MPa275 psiASTM C273
 
Thermal PropertiesMetricEnglishComments
CTE, linear 36.0 µm/m-°C
@Temperature 20.0 °C
20.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Maximum Service Temperature, Air 82.2 °C180 °FContinuous
Minimum Service Temperature, Air -198.3 °C-324.9 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 90.0 °C<= 194 °F
 
Descriptive Properties
Water Absorption0.006 lb/ft²ASTM D2842 at 72°F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HRP - 3/8 - 3.5 Fiberglass/Phenolic Honeycomb
DIAB TBR® 6 Multifunctional Polymer Core Material
DIAB TBR® 10 Multifunctional Polymer Core Material

PDIAB54 / 29831

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.