MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics THERM-A-GAP™ 569 Thermally Conductive Gap Filler Pad
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: THERM-A-GAP™ gap-filler sheets and pads offer excellent thermal properties and highest conformability at low clamping

Features/Benefits: Ultra low deflection force; High thermal conductivity; High tack surface reduces contact resistance; “A” version offers high strength acrylic PSA for permanent attachment; UL recognized V-0 flammability and RoHS compliant

Typical Applications: Telecommunications equipment; Consumer electronics; Automotive electronics (ECUs); LEDs, lighting; Power conversion; Desktop computers; laptops, servers; Handheld devices; Memory modules and Vibration dampening

Product Attributes: Economical combination of thermal performance and conformability

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.20 g/cc2.20 g/ccASTM D792
Thickness 250 - 5000 microns9.84 - 197 mil
Deformation  20 %
@Thickness 3.17 mm,
Pressure 0.0345 MPa
20 %
@Thickness 0.125 in,
Pressure 5.00 psi
0.025 in/min rate; ASTM C165 MOD
 30 %
@Thickness 3.17 mm,
Pressure 0.0689 MPa
30 %
@Thickness 0.125 in,
Pressure 10.0 psi
0.025 in/min rate; ASTM C165 MOD
 50 %
@Thickness 3.17 mm,
Pressure 0.172 MPa
50 %
@Thickness 0.125 in,
Pressure 25.0 psi
0.025 in/min rate; ASTM C165 MOD
 65 %
@Thickness 3.17 mm,
Pressure 0.345 MPa
65 %
@Thickness 0.125 in,
Pressure 50.0 psi
0.025 in/min rate; ASTM C165 MOD
Outgassing - Total Mass Loss 0.42 %0.42 %TML; ASTM E595
Collected Volatile Condensable Material 0.080 %0.080 %ASTM E595
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 1010ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Constant 6.5
@Frequency 1e+6 Hz
6.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 8.00 kV/mm203 kV/inASTM D149
Dissipation Factor <= 0.013
@Frequency 1e+6 Hz
<= 0.013
@Frequency 1e+6 Hz
Chomerics Test
 
Thermal PropertiesMetricEnglishComments
CTE, linear 250 µm/m-°C139 µin/in-°FASTM E831
Specific Heat Capacity 1.00 J/g-°C0.239 BTU/lb-°FASTM D1269
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°FASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 MonthMonths from date of shipment, Aluminum foil; Chomerics
 24.0 Month24.0 MonthMonths from date of shipment, Woven glass; Chomerics
 
Descriptive Properties
CarrierAluminum foil - with PSA
 Woven glass - no PSA
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics THERM-A-GAP™ 579 Thermally Conductive Gap Filler Pad
Parker Chomerics THERM-A-GAP™ HCS10 Thermally Conductive Gap Filler Pad
Parker Chomerics THERM-A-GAP™ G579 Thermally Conductive Gap Filler Pad
Parker Chomerics THERM-A-GAP™ G569 Thermally Conductive Gap Filler Pad
Parker Chomerics THERM-A-GAP™ G515RFA Thermally Conductive Gap Filler Pad

PCHOME311 / 131021

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.