MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Herculoy®, High-Silicon Bronze A, UNS C65500, H02 Temper wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability. Fabricated by blanking, drawing, forming and bending, heading and upsetting, hot forging and pressing, roll threading and knurling, shearing, squeezing, and swaging.

Applications: hydraulic pressure lines, anchor screws, bolts, cable clamps, cap screws, machine screws, marine hardware, nuts, pole-line hardware, rivets, U-bolts, electrical conduits, heat exchanger tubing, welding rod, propeller shafts.

Test specimen: wire - 2mm diameter.

Key Words: HCDA 655, CS101, ISO CuSi3Mn1, CEN CS101, copper-silicon, silicon bronze
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.53 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 675 MPa
Tensile Strength, Yield 395 MPa
@Strain 0.5 %
Elongation at Break 8.0 %In 50 mm
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 30 %UNS C36000 (free-cutting brass) = 100%
Forgeability 40 %UNS C37700 (forging brass) = 100%
Shear Modulus 39.0 GPa
Shear Strength 400 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000246 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 36.0 W/m-K
Melting Point 970 - 1025 °C
Solidus 970 °C
Liquidus 1025 °C
Annealing Point 900 - 1300 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 475 - 700 °C
Hot-Working Temperature 700 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 97 %
Iron, Fe <= 0.80 %
Lead, Pb <= 0.50 %
Manganese, Mn <= 1.5 %
Nickel, Ni <= 0.60 %
Silicon, Si 2.8 - 3.8 %
Zinc, Zn <= 1.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Herculoy®, High-Silicon Bronze A, UNS C65500, H04 Temper wire
Herculoy®, High-Silicon Bronze A, UNS C65500, H01 Temper wire

MC65500d2 / 11669

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.