Adflex KS 084 P is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. Adflex KS 084 P features a high melt flow and a low modulus. It is selected by customers for many commercial and industrial extrusion applications. Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America Application: Carpet Backing; Healthcare Applications; Impact Modification; Roofing Underlayment Market: Flexible Packaging; Industrial, Building & Construction Processing Method: Cast Film; Compounding; Extrusion Coating; Injection Molding Attribute: Good Chemical Resistance; Good Flexibility; Good Heat Seal; Good Puncture Resistance; Good Toughness; Heat Sealable; High ESCR (Environmental Stress Cracking Resistance); High Flow; High Strength; Low Temperature Impact Resistance Information provided by LyondellBasell. |