MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Solus™ 7100 Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Eastman Solus™ 7100 – food contact is a free-flowing powder having low odor and low color. It improves process stability, line speed and paper adhesion of biopolymers in extrusion coating applications. It also allows for downgauging of the coating weight due to the improved adhesion to paper. Eastman Solus 7100 – food contact is based on cellulose, one of the most abundant natural renewable resources. The calculated approximate bio-content value of 49% for Eastman Solus 7100 – food contact was determined by using six bio-based carbon atoms per anhydroglucose unit divided by the total number of carbons per anhydroglucose unit. Although the value reported is not specifically measured for bio-carbon, it can be estimated based on typical partition data.

Applications

  • Packaging component - food contact
  • Paper coatings food packaging
  • Single use articles - food contact
Key Attributes
  • Energy savings in extrusion coating
  • Improved heat sealability
  • Improved processability
  • Reduced coating weight
  • Reduced heat sealing temperature

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/cc
Melt Flow 4.00 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D1238
 
Thermal PropertiesOriginal ValueComments
Melting Point 185 °C
Glass Transition Temp, Tg 159 °C
Decomposition Temperature 267 °COnset
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 3.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4146 / 323769

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.