Hostacom ERC 5022D W95905 is a 20% talc filled PP compounding product. It has good flowablility and stiffness. It is typically used on appliance industry. Availability: Asia-Pacific Application: Appliances Attribute: Good Moldability Information provided by LyondellBasell. |