MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon MAGALA BEM, Pharmaceutical n-Butylethylmagnesium, heptane solutions
Categories: Other Engineering Material

Material Notes: MAGALA BEM is a magnesium alkyl used for disprotonation in organic synthesis.

CAS number: 62202-86-2

EINECS/ELINCS No.: 263-454-0

Applications: MAGALA BEM is used in the manufacture of Ziegler-Natta catalysts for polymerization of olefins.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.726 g/cc0.0262 lb/in³
Viscosity 37.2 cP37.2 cP
 
Thermal PropertiesMetricEnglishComments
Melting Point -42.0 °C-43.6 °F
 
Descriptive Properties
AppearanceClear, colorless to slightly hazy liquid
Content<0.16 wt%Aluminum
 <0.30 wt%Chloride
 4.20-4.60 wt%Magnesium
 40-60 molar%n-Butane
 40-60 molar%Ethane

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY679 / 286202

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.